• 专利标题:   High-stability cathode material used for preparing lithium battery comprises modified porous graphene, modified graphite, mesophase carbon microsphere, lithium titanate, conductive agent and binder.
  • 专利号:   CN112687874-A, CN112687874-B
  • 发明人:   CHEN R, CHEN G, HAN J, LI X, CHEN S, SUN T, CUI G, ZHANG Y, WU H
  • 专利权人:   LUOBEI AOXING NEW MATERIALS CO LTD
  • 国际专利分类:   C01B032/184, C01B032/21, H01M010/052, H01M004/36, H01M004/38, H01M004/485, H01M004/587, H01M004/62
  • 专利详细信息:   CN112687874-A 20 Apr 2021 H01M-004/587 202144 Pages: 9 Chinese
  • 申请详细信息:   CN112687874-A CN11581360 28 Dec 2020
  • 优先权号:   CN11581360

▎ 摘  要

NOVELTY - High-stability lithium battery cathode material comprises 20-30 pts. wt. modified porous graphene, 20-30 pts. wt. modified graphite, 20-30 pts. wt. mesophase carbon microsphere, 20-30 pts. wt. lithium titanate, 5-10 pts. wt. conductive agent and 5-10 pts. wt. binder. USE - The high-stability cathode material is used for preparing lithium battery (claimed). ADVANTAGE - The modified porous graphene has a unique and stable three-dimensional structure. The mesophase carbon microsphere can effectively control the aggravation of the negative polarization, finally obtaining the high-capacity-density and long-life high-stability lithium battery cathode material, and the high-capacity-density and long-life high-stability lithium battery cathode material can still maintain good capacitance under the conditions of high temperature and low temperature, and the capacity retention rate R after circulating for 2000 times at high temperature is higher than 80%. DETAILED DESCRIPTION - INDEPENDENT CLAIMS are included for: (1) application of the high-stability lithium battery cathode material in preparing lithium battery comprising cathode current collector and cathode material coated on the current collector; and (2) preparation of cathode material comprising sequentially weighing modified porous graphene, modified graphite, mesophase carbon microsphere, lithium titanate, conductive agent and binder, mixing uniformly, adding into a ball mill, ball milling, drying, calcining at 850-900 degrees C, cooling, crushing, and sieving.