▎ 摘 要
NOVELTY - A wear-resistant paint comprises 80-100 pts. wt. epoxy modified silicone resin, 15-25 pts. wt. oily acrylic emulsion, 4-7 pts. wt. tert-butylchlorophosphine, 2-5 pts. wt. flaky mica powder, 4-7 pts. wt. propylene glycol methyl ether acetate, 4-7 pts. wt. inositol hexaphosphate, 4-6 pts. wt. diallyl succinate, 1-2 pts. wt. nano-graphene, 3-5 pts. wt. bismaleimide, 10-15 pts. wt. urethane acrylate, 5-7.5 pts. wt. guar gum ether, 8-15 pts. wt. calcined kaolin, 5-10 pts. wt. lead oxide powder, filler, diacetone alcohol, surfactant, preservative formulation and adhesion promoter. USE - Wear-resistant paint for electric vehicle fork. ADVANTAGE - The paint has high fineness, stable anti-aging properties, excellent acid and alkali resistance and salt fog resistance, low surface adhesion, excellent wear resistance and antistatic effect. DETAILED DESCRIPTION - A wear-resistant paint comprises 80-100 pts. wt. epoxy modified silicone resin, 15-25 pts. wt. oily acrylic emulsion, 4-7 pts. wt. tert-butylchlorophosphine, 2-5 pts. wt. flaky mica powder, 4-7 pts. wt. propylene glycol methyl ether acetate, 4-7 pts. wt. inositol hexaphosphate, 4-6 pts. wt. diallyl succinate, 1-2 pts. wt. nano-graphene, 3-5 pts. wt. bismaleimide, 10-15 pts. wt. urethane acrylate, 5-7.5 pts. wt. guar gum ether, 8-15 pts. wt. calcined kaolin, 5-10 pts. wt. lead oxide powder, 5-7.5 pts. wt. filler, 2-5 pts. wt. diacetone alcohol, 0.5-2 pts. wt. surfactant, 5-8 pts. wt. preservative formulation and 1-2 pts. wt. adhesion promoter.