NOVELTY - An automotive interior water-based damping paint comprises 10-20 pts. wt. graphene slurry, 1-3 pts. wt. defoamer, 0.5-1.5 pts. wt. thickener, 50-60 pts. wt. modified glass powder, 3-5 pts. wt. curing agent, 30-40 pts. wt. environment-friendly flame retardant, 60-80 pts. wt. filler, and 2-6 pts. wt. film-forming auxiliary agent. USE - Automotive interior water-based damping paint. ADVANTAGE - The paint solves the problems of prior art, such as low comprehensive performance, complicated preparation process, multiple equipment used and high overall manufacturing cost. DETAILED DESCRIPTION - INDEPENDENT CLAIMS are included for: (1) preparation of the paint comprising weighing raw materials, storing separately, adding modified glass powder and environment-friendly flame retardant to water, grinding to obtain slurry, adding graphene and film-forming auxiliary agent, dispersing, and storing; adding purified water to mixing box, heating to 70 degrees C, adding above prepared mixture, grinding, leaking particles to lower baffle, stirring for 10-15 minutes, adding modified glass powder, stirring for 15-20 minutes, adding defoamer, thickener and curing agent in sequence while stirring for 30-40 minutes, adding environment-friendly flame retardant and filler while stirring for 40-50 minutes, discharging mother liquor through electromagnetic ball valve into homogenizer, and homogenizing for 5-10 minutes; and cooling room temperature, filtering, packaging paint, and storing in clean tank; and (2) paint preparation device comprising mixing box, electric motor, separating plate, baffle plate, and driving shaft.