• 专利标题:   Preparation of graphene-bismuth titanate composite material photocatalyst involves taking bismuth nitrate, adding nitric acid solution, dissolving, taking titanate, adding alcohol solution, mixing, adding prepared solution, and mixing.
  • 专利号:   CN106179311-A
  • 发明人:   XIONG J
  • 专利权人:   XIONG J
  • 国际专利分类:   B01J023/18
  • 专利详细信息:   CN106179311-A 07 Dec 2016 B01J-023/18 201713 Pages: 6 Chinese
  • 申请详细信息:   CN106179311-A CN10513420 20 Nov 2014
  • 优先权号:   CN10513420

▎ 摘  要

NOVELTY - A graphene-bismuth titanate composite material photocatalyst involves preparing graphene according to the Hummers method, dissolving bismuth nitrate in 0-1.5 pH value of nitric acid solution, dissolving, taking titanate, adding alcohol solution, mixing, adding prepared solution, mixing, adding 0.5-2 g of graphene, stirring for 2-4 hours, carrying out hydrothermal reaction, washing with deionized water, and vacuum drying at 350-500 degrees C. USE - Method for preparing graphene-bismuth titanate composite material photocatalyst (claimed). ADVANTAGE - The product has excellent photocatalytic effect.