▎ 摘 要
NOVELTY - Preparing graphene radiation-proof material comprises (a) mixing uniformly graphite, graphene, carbon fiber material (according to mass ratio of 1-2:1-8:1-8 1-8) to obtain mixture; (b) cutting the mixture under condition that the cutting frequency is 3000-50000 revolutions/minute for 1-5 hours; and (c) uniformly stirring the mixture with cyclohexane, silica gel under the condition of 0-80 degrees C, where the mass ratio of the mixture to cyclohexane and silica gel is 1-3:0.20-0.30. USE - The method is useful for preparing graphene radiation-proof material. ADVANTAGE - The method realizes more excellent shielding effect; controls content of impurities in process, batch solves impurity problem, improves working rate of material processing. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for radiation-proof clothes, comprising coating film to the graphene radiation-proof material or spraying or leveling in 15 minutes, and operating at 0-200 degrees C.