NOVELTY - Preparation of porous graphene involves processing biomass-based carbon source with catalyst, obtaining intermediate product (A), heat-preserving intermediate product (A) at 20-40 degrees C and 300-400 degrees C, respectively, obtaining intermediate (B), heat-preserving intermediate (B) at 800-900 degrees C, obtaining intermediate (C), heat-preserving at 1100-1300 degrees C under protective gas atmosphere, obtaining intermediate (D) and heat-preserving intermediate (D) at 900-1000 degrees C. The catalyst is manganese chloride, cobalt compound, nickel compound or iron-based compound. USE - Preparation of porous graphene (claimed). ADVANTAGE - The method enables preparation of porous graphene having high conductivity.