▎ 摘 要
NOVELTY - An environmentally-friendly early strength enriched graphene cement grinding additive comprises 35-55 %mass polymerization polyol, 2-5 %mass acrylate, 3-6 %mass diethylene glycol, 1-3 %mass titanium tetraisopropyl titanate, 3-8 %mass polycarboxylate water-reducing agent, 1-2 %mass calcium dodecylbenzenesulfonate, 1-2 %mass fatty alcohol polyoxyethylene ether sulfate, 5-10 %mass diethanolamine, 5-10 %mass triisopropanolamine, 5 %mass aqueous solution of graphene and remaining industrial waste water. USE - Environmentally-friendly early strength enriched graphene cement grinding additive (claimed). ADVANTAGE - The environmentally-friendly early strength enriched graphene cement grinding additive has improved grinding efficiency, high specific surface area and low sieve residue. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a preparation of environmentally-friendly early strength enriched graphene cement grinding additive.