▎ 摘 要
NOVELTY - Preparing high specific lithium sulfur battery anode material involves using modified hummers method method for preparing graphene oxide material, adding sulfur elementary substance, adding graphene oxide, transferring ultrasonic in ultrasonic cleaner 2-10 hours, putting solution into microwave oven with power is 500-900 watt for 3-15 minutes, treating obtained product with de-ionized water to wash for some times, drying to obtain graphene coating sulfur material. USE - Method for preparing high specific lithium sulfur battery anode material. ADVANTAGE - The method enables to prepare high specific lithium sulfur battery anode material which has potential application value in aspect of energy storage.