▎ 摘 要
NOVELTY - The preparation of graphene conductive fiber involves preparing graphene slurry, coating the core fiber with prepared graphene slurry by coating process to obtain conductive fiber and baking conductive fiber at 150-350 degrees C. USE - Preparation of graphene conductive fiber (claimed). ADVANTAGE - The method enables preparation of graphene conductive fiber with non falling effect, high washability and high durability.