• 专利标题:   Pre-treatment solution used for metal surface, comprises polyfunctional alkyl phosphate, zinc oxide, sodium molybdate, tartaric acid, metal surface oxide, graphene oxide, citric acid and balanced amount of water.
  • 专利号:   CN104988485-A, CN104988485-B
  • 发明人:   GAO X, HOU S, LIU S, MA H, ZHOU K
  • 专利权人:   QINGDAO GERUIXI METAL PROTECTION TECHNOLOGY CO LTD, QINGDAO GERUIXI METAL PROTECTION TECHNOL
  • 国际专利分类:   C23C022/40
  • 专利详细信息:   CN104988485-A 21 Oct 2015 C23C-022/40 201613 Pages: 7 Chinese
  • 申请详细信息:   CN104988485-A CN10425050 20 Jul 2015
  • 优先权号:   CN10425050

▎ 摘  要

NOVELTY - Pre-treatment solution comprises 0.5-1.5 wt.% polyfunctional alkyl phosphate, 2-5 wt.% zinc oxide, 0.5-1 wt.% sodium molybdate, 1-5 wt.% tartaric acid, 1-3 wt.% metal surface oxide, 0.1-0.5 wt.% graphene oxide, 1-2 wt.% citric acid and balanced amount of water. USE - Pre-treatment solution used for metal surface. ADVANTAGE - The pre-treatment solution has corrosion resistance property. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for using pre-treatment solution, which involves: (A) washing the metal surface with acid; (B) soaking the obtained substrate in a pre-treatment solution; and (C) drying the obtained product.