▎ 摘 要
NOVELTY - Seawater corrosion resistant protective agent comprises 30-60 pts. wt. epoxy resin, 20-40 pts. wt. silicone resin, 20-30 pts. wt. anti-corrosion filler, 10-20 pts. wt. graphene, 5-10 pts. wt. bactericide, 5-10 pts. wt. antifoaming agent, 3-8 pts. wt. film-forming auxiliary agent, and 40-60 pts. wt. water. USE - Used as seawater corrosion resistant protective agent. ADVANTAGE - The protective agent combines high flexibility and waterproof performance of silicone resin with high adhesion and excellent corrosion resistance, improves the corrosion resistance, eliminates foam and prevent damage to the appearance of the coating film, prevents the corrosion of protected materials by organisms in seawater, has excellent seawater corrosion resistance, and has no crack and erosion. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for a preparation method of seawater corrosion resistant protective agent, comprising (i) grinding anti-corrosion filler, graphene and a part of water to obtain mixed slurry, and (ii) stirring the mixed slurry with epoxy resin, silicone resin, bactericide, antifoaming agent, film-forming auxiliary agent and remaining amount of water.