▎ 摘 要
NOVELTY - A trans-polyisoprene vulcanizate comprises 0.3-0.7 pt. wt. stearic acid, 5-74 pts. wt. zinc oxide, 0.5-1 pt. wt. accelerator NS, 3-4 pts. wt. sulfur and 0.1-0.9 pt. wt. graphene oxide with respect to 100 pts. wt. trans-polyisoprene. USE - Trans-polyisoprene vulcanizate (claimed). ADVANTAGE - The trans-polyisoprene vulcanizate has excellent mechanical properties by reinforcing polymer with graphene oxide. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of trans-polyisoprene vulcanizate.