▎ 摘 要
NOVELTY - Conductive coating comprises 90-120 pts. wt. matrix resin, 1-9 pts. wt. spherical conductive powder, 0.5-2.7 pts. wt. surfactant, 6-9 pts. wt. dispersant, 40-60 pts. wt. diluent, 20-35 pts. wt. calcium silicate, 15-29 pts. wt. ferric oxide, 2-5 pts. wt. isocyanate curing agent, 1-3.4 pts. wt. glass fiber, 5-8 pts. wt. carbon fluoride, 7-9 pts. wt. carbon fiber, 5-12 pts. wt. graphene, 8-14 pts. wt. aqueous acrylonitrile adhesive and 1-4 pts. wt. UV absorbent. USE - Conductive coating. ADVANTAGE - The coating has improved electrical conductive property and excellent high-temperature resistance.