▎ 摘 要
NOVELTY - A high wearable alloy material comprises 13-25 pts. wt. graphene, 3-8 pts. wt. selenium, 58-63 pts. wt. aluminum powder, 10-13 pts. wt. copper, 4-6 pts. wt. carbon powder, and 3-9 pts. wt. nanocarbon tube. USE - High wearable alloy material. ADVANTAGE - The alloy material has low cost, good wear resistance and strength, and long service life. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a high wear-resistant metal material preparation method which comprises putting each raw material into mixer to carry out mixing, heating at 100-150 degrees C/hour to 3890 degrees C, cooling to 1000 degrees C at 230-250 degrees C/hour, and keeping temperature for 2-3 hours; and cooling to room temperature, heating alloy material, annealing, insulating for 2-3 hours at 590 degrees C, and air cooling to room temperature.