▎ 摘 要
NOVELTY - Preparation of graphene quantum dot/tin sulfide nanosheet composite photocatalyst comprises measuring 1-6 ml graphene quantum dots, adding distilled water, weighing 2-25 mmol sulfur source and 1-10 mmol tin tetrachloride, mixing for 30 minutes, charging reaction kettle, heating at 120-180 degrees C for 4-24 hours, cooling to room temperature, centrifuging and drying precipitate for 6 hours. USE - Method of preparing graphene quantum dot/tin sulfide nanosheet composite photocatalyst (claimed). ADVANTAGE - The method has simple operation, mild condition and high yield.