▎ 摘 要
NOVELTY - Modified thermoplastic hollow polymer microsphere, comprises oil phase, a water phase and graphene oxide, where mass ratio of water phase and oil phase is (1-4): (6-9). USE - Modified thermoplastic hollow polymer microsphere used for aqueous coating. ADVANTAGE - The modified thermoplastic hollow polymer microspheres have good particle size uniformity, good solvent resistance and high foaming ratio. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing a modified thermoplastic hollow polymeric microsphere, which involves: uniformly mixing the oil phase and the water phase, reacting to obtain the thermoplastic hollow polymer microspheres, and mixing and reacting with the graphene oxide dispersion liquid to obtain modified thermoplastic hollow polymer microspheres.