▎ 摘 要
NOVELTY - Anti-corrosive coating comprises 70-76 pts. zinc powder, 3.6-3.8 pts. cyclohexanone, 3.6-3.8 pts. ethylene glycol butyl ether, 0.20-0.22 pts. graphene, 15-15.5 pts. epoxy resin, 0.16-0.18 pts. organobentonite, 0.05-0.06 pts. anhydrous ethanol and 1.40-1.50 pts. xylene. USE - Used as an anti-corrosive coating. ADVANTAGE - The method is simple and suitable for industrial production. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing coating, comprising: (a) mixing xylene and organic bentonite by stirring for first time, then adding anhydrous ethanol and stirring for second time to obtain a first mixture; (b) mixing cyclohexanone, ethylene glycol butyl ether and 0.24-0.26 pts. anti-settling agent by stirring, sequentially adding zinc powder, graphene slurry and epoxy resin into above mixture and stirring to obtain a second mixture; (c) mixing the first mixture and second mixture by stirring to obtain a third mixture; and (d) adding 0.05-0.15 pts. defoamer and leveling agent into the third mixture and stirring.