▎ 摘 要
NOVELTY - The brick has a brick body formed by combination of part of potassium feldspar, 45 parts of spodumene, 20 parts of guangxi white mud, 15-20 parts of attapulgite, 30-50 parts of corundum, 2-30 parts of water, 30-50 parts of graphite, 1-3 parts of trimeric sodium phosphate and 1-2 parts of steel fiber. A glaze spraying unit is fixed on an upper part of a blank surface. Sintering temperature is about 1195-1205 degrees centigrade. A graphene enhance ceramic tile finished product is obtained in firing period to perform subsequent processing operation. USE - Graphene enhance ceramic brick. ADVANTAGE - The brick has high mechanical strength.