• 专利标题:   Graphite radiating copper foil paint comprises graphene slurry, boron slurry, bonding agent and diluent, where graphene slurry comprises graphene powder, surface treating agent and solvent, and has improved radiating performance.
  • 专利号:   CN107916041-A
  • 发明人:   DING X, ZONG Y, WANG D
  • 专利权人:   SHENZHEN GUOCHUANG JIAWEI GRAPHENE TECHN
  • 国际专利分类:   B32B015/01, C09D133/04, C09D163/00, C09D007/62
  • 专利详细信息:   CN107916041-A 17 Apr 2018 C09D-133/04 201833 Pages: 8 Chinese
  • 申请详细信息:   CN107916041-A CN11341700 14 Dec 2017
  • 优先权号:   CN11341700

▎ 摘  要

NOVELTY - Graphite radiating copper foil paint comprises 5-30 pts. wt. graphene slurry, 25-70 pts. wt. boron slurry, 5-10 pts. wt. bonding agent and 1-60 pts. wt. diluent. The graphene slurry comprises 5-50 pts. wt. graphene powder, 1-10 pts. wt. surface treating agent and 40-94 pts. wt. solvent. The boron nitride slurry comprises 10-30 pts. wt. boron nitride powder, 1-10 pts. wt. surface processing agent and 60-89 pts. wt. solvent. USE - Graphite radiating copper foil paint. ADVANTAGE - The graphite radiating copper foil paint has improved radiating and insulating performance. DETAILED DESCRIPTION - Graphite radiating copper foil paint comprises 5-30 pts. wt. graphene slurry, 25-70 pts. wt. boron slurry, 5-10 pts. wt. bonding agent and 1-60 pts. wt. diluent. The graphene slurry comprises 5-50 pts. wt. graphene powder, 1-10 pts. wt. surface treating agent and 40-94 pts. wt. solvent. The boron nitride slurry comprises 10-30 pts. wt. boron nitride powder, 1-10 pts. wt. surface processing agent and 60-89 pts. wt. solvent. The surface treatment agent includes one or more amides and polyethers. The solvent is propylene glycol methyl ether acetate, methyl nylon acetate, toluene and butyl acrylate. The binder is an acrylic resin, epoxy resin or a silicone resin. The diluent is one or more of ethylene glycol, ethylene glycol butyl ether acetate or butyl acetate or propylene glycol methyl ether acetate. An INDEPENDENT CLAIM is included for a method for preparing graphite radiating copper foil paint, which involves: (A) mixing 1-60 pts. wt. diluent, 1-10 pts. wt. surface treatment agent and 30-80 pts. wt. graphite alkene powder; (B) stirring the mixture; (C) carrying out sand grinding or ball milling to obtain graphene slurry; (D) adding 1-60 pts. wt. diluent, 1-10 pts. wt. surface processing agent and 20-70 pts. wt. boron nitride; (E) stirring the obtained mixture; (F) carrying out sand grinding or ball milling to obtain the boron nitride slurry; (G) mixing and stirring graphene slurry and boron slurry; and (H) adding bonding agent.