▎ 摘 要
NOVELTY - Rubber comprises 100 pts. wt. natural rubber, 0.2-1 pt. wt. stearic acid, 2-10 pts. wt. zinc oxide, 0.1-1 pts. wt. accelerator, 0-0.3 pts. wt. retarder N-(cyclohexylthio) phthalimide, 1-5 pts. wt. sulfur, and 0.1-1 pts. wt. graphene oxide. USE - Rubber. ADVANTAGE - The rubber has low cost and scorch time. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of rubber comprising taking natural rubber in open mill, refining machine at 70 plus minus 5 degrees C degrees C and cooling; rolling for 1-5 times; adjusting distance to 0.5-1.5 mm using film bag roller, and regulating roller distance to 1.5-2 mm for 3-5 minutes; adding graphene oxide, and rolling for 2-4 minutes for 3-5 times; adding other raw materials, rolling for 2-5 minutes, and cutting; and taking capsule material.