▎ 摘 要
NOVELTY - An improving water solubility nanomaterial is prepared by ultrasonically dissolving nano granule in cyclohexane or chloroform for 5-30 minutes, adding graphene oxide derivative for 40-480 seconds, centrifugally separating at 14800-20000 revolutions/minute, washing with water, and drying. USE - Method for preparing improving water solubility of nanomaterial (claimed). ADVANTAGE - The nanomaterial has good water solubility and versatility.