• 专利标题:   Clothing fabric comprises a warp yarn and a weft yarn, formed by weaving, where the warp yarn comprises graphene oxide, Modal fiber, glass fiber, bamboo charcoal fiber, copper fiber and nano-alumina.
  • 专利号:   CN107190398-A
  • 发明人:   UNANNOUNCED I
  • 专利权人:   HEFEI BUZHU MENGYI CLOTHING TRADE CO LTD
  • 国际专利分类:   D03D001/00, D03D013/00, D03D015/00, D06M101/06, D06M101/12, D06M101/40, D06M013/224, D06M015/564
  • 专利详细信息:   CN107190398-A 22 Sep 2017 D03D-015/00 201779 Chinese
  • 申请详细信息:   CN107190398-A CN10629121 28 Jul 2017
  • 优先权号:   CN10629121

▎ 摘  要

NOVELTY - Clothing fabric comprises a warp yarn and a weft yarn, formed by weaving. The warp yarn comprises 3-4 pts. graphene oxide, 40-50 pts. Modal fiber, 1-2 pts. glass fiber, 10-12 pts. bamboo charcoal fiber, 0.5-0.8 pts. copper fiber and 2-4 pts. nano-alumina. The weft yarn comprises 0.2-0.4 pts. tourmaline, 4-5 pts. soybean fiber, 1-2 pts. aluminum hydroxide, 15-20 pts. carbon fiber and 15-18 pts. wool fiber. The polyurethane layer comprises polyurethane resin, toluene, butanone, curing agent, ultraviolet absorber, castor oil, mustard and flavor. USE - Used as clothing fabric. DETAILED DESCRIPTION - Clothing fabric comprises a warp yarn and a weft yarn, formed by weaving. The warp yarn comprises 3-4 pts. graphene oxide, 40-50 pts. Modal fiber, 1-2 pts. glass fiber, 10-12 pts. bamboo charcoal fiber, 0.5-0.8 pts. copper fiber and 2-4 pts. nano-alumina. The weft yarn comprises 0.2-0.4 pts. tourmaline, 4-5 pts. soybean fiber, 1-2 pts. aluminum hydroxide, 15-20 pts. carbon fiber and 15-18 pts. wool fiber. The warp and weft surfaces are provided with a polyurethane layer. The polyurethane layer comprises 100 pts. polyurethane resin, 1-2 pts. toluene, 3-4 pts. butanone, 2-6 pts. curing agent, 0.2-0.8 pts. ultraviolet absorber, 3-4 pts. castor oil, 1-2 pts. mustard and 1-2 pts. flavor. An INDEPENDENT CLAIM is also included for manufacturing clothing fabric, comprising: (i) adding the warp and weft into the reaction kettle, melting individually, then adding rayon; (ii) freezing the warp and weft in a refrigerator for 5-10 minutes; (iii) soaking the warp yarn and weft yarn in polyurethane solution for 10-20 minutes, taking out and drying; and (iv) weaving the warp and weft yarn into fabric via weaving machine.