• 专利标题:   Bone china porcelain tea set comprises graphene, carbon nanotubes, kieselguhr, kaolin, feldspar, bone charcoal, spodumene, pyrophyllite, deep sea shell powder, quartz and silicon nitride as raw materials.
  • 专利号:   CN108675766-A
  • 发明人:   WU Y, WU C, QI L
  • 专利权人:   ZHEJIANG NAVIION TECHNOLOGY CO LTD
  • 国际专利分类:   C04B033/135, C04B033/36, C04B041/86, C03C008/00, A47G019/22
  • 专利详细信息:   CN108675766-A 19 Oct 2018 C04B-033/135 201880 Pages: 8 Chinese
  • 申请详细信息:   CN108675766-A CN10569788 05 Jun 2018
  • 优先权号:   CN10569788

▎ 摘  要

NOVELTY - Bone china porcelain tea set comprises 1-20 pts. wt. graphene, 1-30 pts. wt. carbon nanotubes, 1-2 pts. wt. kieselguhr, 400-600 pts. wt. kaolin, 50-100 pts. wt. feldspar, 20-400 pts. wt. bone charcoal, 1-50 pts. wt. spodumene, 1-80 pts. wt. pyrophyllite, 1-4000 pts. wt. deep sea shell powder, 1-100 pts. wt. quartz and 1-40 pts. wt. silicon nitride as raw materials. USE - Bone china porcelain tea set. ADVANTAGE - The bone china porcelain tea set has good heat resistance and cold resistance, good toughness, and health protection function to human body. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for constructing a ion bone china porcelain tea set, which involves: (A) taking porcelain stone and crush it, and washing out the magazine to precipitate, and than adding water to adjust the mud to remove the slag; (B) extruding the air in the mud mass and distributing the moisture in the mud, and adding functional materials to the weight ratio of the blank; (C) crushing the glaze and stone, than add water to the weight ratio of black glaze, white glaze and azure glaze formula; (D) stirring, and kneading in sequence, and perform the mixing, and then performing hydrophobic water, and measuring fineness and concentration, and drying the blank, placing the processe ceramic blank on the rack to dry; and (E) burning the kiln, applying glaze and baking at suitable conditions to obtain the desired product.