▎ 摘 要
NOVELTY - A rubber emulsion condensate comprises 100 pts. wt. rubber latex, 1-40 pts. wt. emulsified oil, 1-20 pts. wt. graphene oxide suspension and 0.1-5 pts. wt. antioxidant. USE - Rubber emulsion condensate (claimed). ADVANTAGE - The rubber emulsion condensate has high tensile strength and reinforcement property, and excellent wear resistance, and is prepared by simple, economical, easy and economical method. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of rubber emulsion condensate, which involves graphene oxide suspension, adding antioxidant and rubber latex, reacting at 30-60 degrees C for 10-30 minutes, adding emulsified oil, stirring for 1-10 minutes, adding flocculating agent and dehydrating by drying.