▎ 摘 要
NOVELTY - Preparation of graphene aerogel comprises preparing polyvinyl alcohol aqueous solution containing graphene oxide, obtaining graphene dispersion liquid with concentration of 1-10 mg/cm3, freezing at not greater than - 196 degrees C to obtain frozen sample, freeze-drying to obtain freeze-dried sample, performing high-temperature reduction at 350-450 degrees C for 2-3 hours under mixed gas atmosphere of argon and hydrogen, and burning at 900-1100 degrees C for 2-3 hours. USE - Method for preparing graphene aerogel (claimed). ADVANTAGE - The aerogel has stable and uniform structure.