▎ 摘 要
NOVELTY - The preparation method of composite conductive material involves adding graphene oxide and water to alcohol solvent and then mixing, adding stannous chloride dihydrate and antimony pentachloride to the mixture and then stirring, adding urea to the mixture and then stirring, hydrothermally reacting the mixture at 100-200 degrees C for 12-18 hours and then centrifugally separating, and calcining at high temperature. USE - The method is useful for preparation of composite conductive material (claimed). ADVANTAGE - The method enables simple preparation of composite conductive material with high yield and excellent electrical conductivity. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for composite conductive material prepared by the method.