• 专利标题:   Central heating pipe wall anti-corrosion coating comprises e.g. fluorinated epoxy resin, epoxy resin, titanium dioxide, fine silica powder, graphene, teflon wax, amino resin, mixed solvent, polyamide curing agent and mixed solvent.
  • 专利号:   CN107502135-A
  • 发明人:   LI S, LIU M, HUANG Y, ZHANG X, FAN J, QU W
  • 专利权人:   SHANDONG WOFENG GREENWORLD TUBE CO LTD, UNIV QINGDAO SCI TECHNOLOGY
  • 国际专利分类:   C09D127/18, C09D161/20, C09D163/00, C09D005/08
  • 专利详细信息:   CN107502135-A 22 Dec 2017 C09D-163/00 201808 Pages: 6 Chinese
  • 申请详细信息:   CN107502135-A CN10701547 16 Aug 2017
  • 优先权号:   CN10701547

▎ 摘  要

NOVELTY - Central heating pipe wall anti-corrosion coating comprises component A including 30-40 pts. wt. fluorinated epoxy resin, 40-60 pts. wt. epoxy resin, 30-50 pts. wt. titanium dioxide, 5-10 pts. wt. ultra-fine sericite, 8-16 pts. wt. fine silica powder, 1-5 pts. wt. graphene, 10-20 pts. wt. teflon wax, 3-8 pts. wt. amino resin, 10-30 pts. wt. mixed solvent, 2-5 pts. wt. dispersant, 0.2-0.6 pts. wt. defoamers and 0.2-0.5 pts. wt. leveling agent; and component B including 50 pts. wt. polyamide curing agent and 50 pts. wt. mixed solvent. USE - Used as central heating pipe wall anti-corrosion coating. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparation of central heating pipe wall anti-corrosion coating comprising (i) dispersing the components of component A at 1500-2500 revolutions per minute with a disperser for 1 hour, and then grinding the mixed material fineness less than or equal to 20 mu m and packaging to obtain component A, (ii) dispersing the components of component A at 1500-2500 revolutions per minute with a disperser for 0.5 hour, stirring for 0.5 hours and packaging to obtain component B, and (iii) mixing obtained component A and component B in a weight ratio of 8-12:1 to obtain final product.