▎ 摘 要
NOVELTY - Electromechanical equipment processing coolant comprises 60-90 pts. wt. deionized water, 30-46 pts. wt. ethylene glycol, 10-14 pts. wt. dimethyl silicone oil, 12-18 pts. wt. oxidized graphene powder, 8-13 pts. wt. sodium molybdate, 5-9 pts. wt. sorbitol, 7-11 pts. wt. methyl orthosilicate, 4-12 pts. wt. cellulose ether, 5-8 pts. wt. alcohol amine, 5-11 pts. wt. polyethylene alcohol, 6-13 pts. wt. nano-silica, 5-9 pts. wt. absolute ethanol, 1-5 pts. wt. organic additive and 2-6 pts. wt. coolant. USE - Electromechanical equipment processing coolant. ADVANTAGE - The electromechanical equipment processing coolant is scientific, improves the cooling property, has good cooling performance, good anti-freezing effect, is non-corrosive and does not pollute the cooling pipeline. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing electromechanical equipment processing coolant, which involves: (A) introducing deionized water into a mixing kettle, and heating mixing kettle at 25-45 degrees C, and the stirring; (B) adding ethylene glycol, dimethicone, graphene oxide powder, sodium molybdate, sorbitol, orthosilicate ester, cellulose ether, alcohol amine, polyvinyl alcohol, nano silica, absolute ethanol, stirring for 30-40 minutes to obtain a stirred mixture; (C) stirring mixture, adding organic additives and coolant, stirring for 50-80 minutes; and (D) sampling test, qualified, filling to get desired coolant.