▎ 摘 要
NOVELTY - Producing graphene garment material comprises (i) stirring 25-45 wt.% graphene nano-material, 35-55 wt.% cotton fabric carrier, 6-10 wt.% sulfonate powder, 8-13 wt.% chitosan with deacetylation degree of 10-18% and 15-30 wt.% anions for 1-3 hours to obtain mixed raw material, (ii) placing the mixed raw material in the pulping machine, pumping through a slurry tank, drying in oven for 40-80 minutes and collecting 600-800 meshes of graphene garment material raw powder and (iii) dissolving graphene garment material raw powder in deionized water to obtain 0.3 mg/ml electrolyte solution, stirring or ultrasonically treating and dissolving the electrolyte to obtain uniformly mixed solution. USE - The graphene garment material is useful for producing autumn and winter exterior/autumn and winter underwear (claimed). ADVANTAGE - The garment material has good air permeability, strong antibacterial effect, good warmth and anti-static effect; and releases far infrared ray and has moisture absorption property. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for the graphene garment material, comprising graphene nano-material, cotton fabric carrier, sulfonate powder, chitosan and anion, where the cotton fabric carrier comprises either 30-50 pts. wt. garment material, 10-20 pts. wt. polyvinyl chloride powder with a fineness of 0.2-1.2 nm, 15-20 pts. wt. dibutyl phthalate, 0.04-0.08 pts. wt. zinc stearate and 0.1-0.3 pts. wt. glycerol, or 0-60 pts. wt. garment material, 10-30 pts. wt. polyvinyl chloride powder with a fineness of 0.1-0.9 nm, 10-29 pts. wt. dibutyl phthalate, 0.06-0.1 pts. wt. zinc stearate and 0.4-0.7 pts. wt. glycerol.