▎ 摘 要
NOVELTY - Nanocomposite graphene modified mine supporting roller pipe material comprises 4-6 pts. wt. nano super-conductive carbon black, 5-8 pts. wt. polyethylene and acrylic acid graft copolymer, 3-5 pts. wt. graphene, 3-5 pts. wt. micropowder graphite, 4-6 pts. wt. ultrafine microcapsule red phosphorus, 8-10 pts. wt. nanomagnesium hydroxide, 3-5 pts. wt. ammonium polyphosphate, 3-5 pts. wt. organic montmorillonite, 1-3 pts. wt. white carbon black, 0.2-1 pts. wt. coupling agent, 0.5-2 pts. wt. antioxidant, 3-5 pts. wt. carbon forming agent, 3-5 pts. wt. dispersant, 0.2-0.3 pts. wt. zinc stearate and 60-80 pts. wt. ultra-high molecular weight polyethylene. USE - Used as nanocomposite graphene modified mine supporting roller pipe material. ADVANTAGE - The material is tested and analyzed to meet the requirements of the mining roller pipe body. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the material. DESCRIPTION OF DRAWING(S) - The drawing shows a schematic view of magnetic fluid stirring device.