▎ 摘 要
NOVELTY - A corrosion resistant material comprises 30-100 pts. wt. carbon fiber, 20-80 pts. wt. flame-retardant viscose adhesive, 1-10 pts. wt. nano titanium dioxide, 0.5-5 pts. wt. lubricant, 2-50 pts. wt. nylon fiber, 0.01-0.1 pt. wt. alkyd resin, 2-15 pts. wt. toughener and 15-60 pts. wt. graphene carbon nanotube slurry. The graphene carbon nanotube slurry has 30-50 mg/mL carbon nanotube and 2-3 mg/mL graphene. USE - Corrosion resistant material used for protective clothing (claimed). ADVANTAGE - The product is flexible and oil proof, has long service life and meets special use environment conditions.