▎ 摘 要
NOVELTY - Graphene heating paint comprises 40-50 wt.% graphene, 5-14 wt.% oxide, 20 wt.% aqueous resin, 20-30 wt.% adhesive, 0.1-0.5 wt.% antifoaming agent, 0.3-0.5 wt.% coupling agent and 0.3-0.5 wt.% flatting agent. USE - Used as graphene heating paint. ADVANTAGE - The graphene heating paint has high electrothermal conversion rate, rapid heating, long service life, and uniform heating temperature; can be directly roller coated or sprayed on walls, floors and other locations which improve energy efficiency and save more energy and electricity than traditional heating methods. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing graphene heating paint comprising (i) crushing the oxide into powder and passing through a sieve with a mesh number of 500-2000 mesh, (ii) adding oxide to the reaction kettle, adding aqueous resin, graphene, binder, antifoaming agent, coupling agent and flatting agent and stirring uniformly, (iii) grinding the slurry uniformly stirred in step (ii) by grinder to obtain slurry having a particle size of 80-100 mu m, and (iv) adding deionized water of 40-60% of the slurry weight to adjusting the consistency to obtain final product.