▎ 摘 要
NOVELTY - Powerful antioxidant fast drying paint comprises 40-50 pts. wt. acrylic resin, 6-12 pts. wt. epoxy resin, 2-3 pts. wt. graphene, 8-12 pts. wt. butyl acetate, 2-4 pts. wt. polylactide, 4-8 pts. wt. silicone oil, 3-6 pts. wt. zinc oxide, 1-2 pts. wt. titanium dioxide, 1.6-2.8 pts. wt. thiodipropionate diester, 2-2.6 pts. wt. rosin pentaerythritol ester, 1.4-1.6 pts. wt. leveling agent and 0.6-1.4 pts. wt. defoaming agent. USE - Used as powerful antioxidant fast drying paint. ADVANTAGE - The paint: has high anti-oxidation performance, high film thickness, strong protective effect, and reduced labor cost. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing powerful antioxidant fast drying paint comprising (i) mixing acrylic resin and epoxy resin, taking 1 pts. wt. deionized water, heating at 50-55 degrees C, pouring the mixed resin into deionized water and stirring at constant speed for 40-60 minutes to obtain mixed resin, (ii) pouring butyl acetate, polylactide, silicone oil, thiodipropionate diester and rosin pentaerythritol ester into blender and mixing to obtain mixed slurry, (iii) mixing graphene, zinc oxide and titanium dioxide, placing in dispersion cylinder together with mixed resin, stirring for 30-40 minutes, pouring leveling agent and defoaming agent into dispersion tank, stirring for 60-70 minutes, (iv) pouring mixed slurry in step (ii) into dispersion tank in step (iii), raising temperature to 35-40 degrees C and stirring at constant speed for 2-3 hours to obtain final product.