▎ 摘 要
NOVELTY - A biomass graphene fabric comprises a surface coating layer and five three-strand satin fabric bases composed of silver fiber warp yarns and olefinic biomass fiber weft yarns, where the surface coating layer comprises 33-65 pts. wt. dihydroxypolydimethylsiloxane, 18-25 pts. wt. hydroxypolydimethylsiloxane, 22-26 pts. wt. acrylic resin, 3-6 pts. wt. methyl tributyl ketone silane, 1-3 pts. wt. aminopropyl trimethoxy silane, 1-2 pts. wt. tetrabutyl titanate, 3-5 pts. wt. hydroxypropyl acrylate, 17-20 pts. wt. nano titanium dioxide, 2-4 pts. wt. 1,3-dimethyl-2-imidazolidinone, 2-3 pts. wt. sodium benzenesulfinate and 2-6 pts. wt. glycidyl methacrylate. USE - Biomass graphene fabric. ADVANTAGE - The biomass graphene fabric has excellent antibacterial effect. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for a method for preparing a biomass graphene fabric, which involves interlacing the silver fiber warp yarn and the olefinic biomass fiber weft yarn to obtain a fabric, pouring 33-65 pts. wt. dihydroxypolydimethylsiloxane, 18-25 pts. wt. hydroxypolydimethylsiloxane, 22-26 pts. wt. acrylic resin, 3-6 pts. wt. methyl tributyl ketone silane, 1-3 pts. wt. aminopropyl trimethoxy silane, 1-2 pts. wt. tetrabutyl titanate, 3-5 pts. wt. hydroxypropyl acrylate, 17-20 pts. wt. nano titanium dioxide, 2-4 pts. wt. 1,3-dimethyl-2-imidazolidinone, 2-3 pts. wt. sodium benzenesulfinate and 2-6 pts. wt. glycidyl methacrylate into a reaction kettle for mixing and stirring treatment, the stirring speed of the mixing and stirring treatment is 40-60 rpm/minutes for 1-2 hours to obtain the finished product.