▎ 摘 要
NOVELTY - Preparing conductive organosilicone involves slowly adding vinyl-terminated silanized graphene oxide suspension to hydrogen-containing silicone oil emulsion, adding catalyst chloroplatinic acid, heating at 60-80 degrees C, reacting for 2-8 hours, filtering, washing with toluene to remove hydrogen-containing silicone oil that is not reacted with graphene oxide, and vacuum drying. The mass ratio of hydrogen-containing silicone oil emulsion, vinyl-terminated silanized graphene oxide suspension and chloroplatinic acid is 100:(30-70):(0.5-2). USE - The method is useful for preparing conductive organosilicone. ADVANTAGE - The method provides conductive organosilicone with high conductivity of 10-2 to 103 S/cm, and connects conductive graphene oxide to organosilicone polymer chain segment by covalent bonding.