▎ 摘 要
NOVELTY - Anti-static finishing solution comprises 10-12 g/l graphene oxide, 5-8 g /l anhydrous sodium carbonate, 10-20 g/l methacrylic acid resin, 10-20 g/l sodium chloride,10-15 g/l ammonium persulfate, 3-4 drops of fatty alcohol polyoxyethylene ether, and water as solvent. USE - Used as anti-static finishing solution containing graphene oxide (claimed). ADVANTAGE - The finishing solution: achieves the anti-static effect; and improves the charge quantity of the materials. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the anti-static finishing solution of graphene, comprising (i) taking the fabric to-be-treated, placing in the cleaning agent, processing for 60-80 minutes, wet by the clean water and drying, (ii) according to the bath ratio of 1:50-100, placing the finishing liquor at 90-100 degrees C of water bath, placing the fabric finishing liquid, dipping for 10-12 minutes, washing by using clean water, and drying, (iii) adding witch hazel distillate, raising the temperature to 40 to 50 degrees C, reacting for 20-30 minutes, washing by using clean water, and drying.