▎ 摘 要
NOVELTY - Fluorinated graphene modified fluororesin coating comprises 1-20 wt.% fluorine resin, 0.1-1 wt.% fluorinated graphene, 20-99 wt.% fluorine solvent, and 2-20 wt.% organic solvent. USE - Used as Fluorinated graphene modified fluororesin coating. ADVANTAGE - The method: is simple, and convenient for industrial production. The coating: significantly enhances the hydrophobic and oleophobic ability of fluororesin. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the fluorinated graphene modified fluororesin coating, comprising mixing fluorine resin with fluorine solvent, mechanically stirring for 3-6 hours to obtain a fluorine resin solution, mixing fluorinated graphene with organic solvents, ultrasonically dispersing at room temperature for 10-30 minutes to obtain a fluorinated graphene dispersion liquid, mixing the fluorine resin solution with the fluorinated graphene dispersion liquid, and ultrasonically dispersing for 10-30 minutes.