▎ 摘 要
NOVELTY - A transition metal sulfides/graphene nanocomposite is prepared by mixing sulfur compound and 0.5-10% graphene powder, grinding for 20-40 minutes, adding transition metal salt, grinding for 30-60 minutes, heating at 50-200 degrees C for 3-80 minutes, washing, and drying. USE - Method for preparing transition metal sulfides/graphene nanocomposite (claimed). ADVANTAGE - The nanocomposite has low synthesis temperature, low cost and good dispersion uniformity.