▎ 摘 要
NOVELTY - Graphene film forming agent comprises 0.11-0.21 wt.% modified graphene, 0.03-0.06 wt.% graphene oxide, 0.2-0.4 wt.% citric acid, 0.1-0.3 wt.% tartaric acid, 0.2-0.4 wt.% sodium fluoroborate, 0.8-1.6 wt.% complex, 0.8-1.0 wt.% fluoride and balance deionized water. USE - Graphene film forming agent. ADVANTAGE - The product has good corrosion resistance and good adhesion property. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of graphene film forming agent comprising adding 1/5-1/4 water into the reactor, adding modified graphene and graphene oxide, stirring for 5-6 hours, adding citric acid, tartaric acid and sodium fluoroborate, stirring for 1-2 hours, adding fluoride, stirring for 0.5-1 hour, adding complex, stirring for 2-3 hours, adding the remaining water and stirring.