▎ 摘 要
NOVELTY - Preparation of hybrid proton exchange membrane comprises dispersing graphene oxide in water-organic solvent solution, sealing with aluminum foil paper at 15-65 degrees C to carry out adsorption, evaporating for 0.5-2400 hours, removing aluminum foil, pouring graphene oxide on aluminum foil to react at 0.7-0.95 atm, standing for 1-120 minutes, heating slowly to remove solvent, vacuumizing for 12-36 hours, taking out aluminum foil and soaking in acid-hydrogen peroxide solution. USE - Method for preparing hybrid proton exchange membrane (claimed). ADVANTAGE - The method has simple operation process, mild preparation condition, low production cost and easy mass production.