▎ 摘 要
NOVELTY - Composition comprises 90-110 pts. wt. polyether polyol, 85-100 pts. wt. isocyanate, 1-5 pts. wt. catalyst, 1-5 pts. wt. foaming agent, 5-10 pts. wt. foam stabilizer, 0.5-2 pts. wt. nitrogen-doped graphene, 0.5-1.5 pts. wt. modified indianite nanotube and 1-3 pts. wt. cellulose nanocrystals. USE - The method is useful for preparing the positioning pad (claimed). DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the positioning pad from the composition, comprising (i) mixing the composition to obtain a mixture and (ii) adding the mixture obtained in the step (i) into a mold to be solidified, and obtaining the positioning pad.