▎ 摘 要
NOVELTY - Preparation of compression tile comprises crushing and sieving steel slag to obtain steel slag powder; mixing 40-50 pts. wt. steel slag, 20-30 pts. wt. epoxy resin, 5-6 pts. wt. curing agent, 10-20 pts. wt. xanthan gum solution, 10-20 pts. wt. peach gum solution, 20-30 pts. wt. cement, 10-20 pts. wt. fly ash, 20-30 pts. wt. oxidized graphene powder, 10-20 pts. wt. modified starch emulsion, 10-20 pts. wt. talc powder, 10-20 pts. wt. urea, 60-80 pts. wt. of water, stirring and mixing to obtain mixed slurry; injection molding the mixed slurry, compression molding, and demolding to obtain molded blank; and immersing the shaped blank in Bacillus solution, taking out and drying. USE - Method for preparing compression tile used as building material. ADVANTAGE - The prepared tile has excellent mechanical property.