• 专利标题:   Heat dissipation anticorrosive coating comprises macromolecular resin synthetic material, dispersing agent, pigment, graphene, flatting agent, filler, antifoaming agent, thickening agent, flatting powder and deionized water.
  • 专利号:   CN113061360-A
  • 发明人:   XU B, ZHONG Y
  • 专利权人:   DONGGUAN PENGWEI ENERGY TECHNOLOGY CO LT
  • 国际专利分类:   C09D001/00, C09D127/18, C09D181/06, C09D183/04, C09D005/08, C09D007/61
  • 专利详细信息:   CN113061360-A 02 Jul 2021 C09D-005/08 202163 Pages: 5 Chinese
  • 申请详细信息:   CN113061360-A CN10333302 29 Mar 2021
  • 优先权号:   CN10333302

▎ 摘  要

NOVELTY - Heat dissipation anticorrosive coating comprises 60-70 wt.%. macromolecular resin synthetic material, 2-5 wt.%. dispersing agent, 3-5 wt.%. pigment, 5-10 wt.%. graphene, 0.3-0.5 wt.%. flatting agent, 5-10 wt.%. filler, 0.1-0.3 wt.%. antifoaming agent, 1-2 wt.%. thickening agent, 2-5 wt.%. flatting powder and 8-12 wt.%. deionized water. USE - Used as heat dissipation anticorrosive coating comprising e.g. macromolecular resin synthetic material. ADVANTAGE - The heat dissipation anticorrosive coating has smooth surface, high hardness, high wear resistance, high temperature resistance, corrosion resistance, excellent thermal conductivity, excellent anti-corrosion performance and fast heat dissipation performance; protects heating components; prolongs the service life; has good effect, heat resistance and provides excellent protection effect. The method has no volatile organic components emissions; is pollution-free and stimulation-free. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing heat dissipation anticorrosive coating comprising adding the macromolecular resin synthetic material and dispersing agent to a dispersing kettle, dispersing at a speed of 300-500revolutions/minutes for 3-5 minutes, adding graphene, pigments, fillers and flatting powder in the dispersion, dispersing at a speed of 2000-3000revolutions/minutes for 60 minutes, reducing the speed to 300-500revolutions/minutes, adding flatting agent, antifoaming agent and thickening agent, adjusting the viscosity with deionized water, dispersing for 10 minutes, filtering and packaging to obtain the finished product coating, where the color is light ash to black.