▎ 摘 要
NOVELTY - Low surface energy antifouling coating comprises a nano material, a monomer, an initiator, and a solvent. A mass ratio of the monomer to the nano material and the initiator is 1:(0.01-0.05):(0.002-0.008). The nano material is selected from at least one of graphene, carbon nanotubes, and hexagonal boron nitride. The monomer includes 8-18 wt.% of a silicon monomer, 12-20 wt.% of a fluorine monomer, 30-40 wt.% of an epoxy resin monomer and 30-40 wt.% of acrylic resin monomer. USE - Low surface energy antifouling coating. ADVANTAGE - The low surface energy antifouling coating has good binding force with excellent corrosion resistance and abrasion resistance, and has the function of self-repair of corrosion. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing a low surface energy antifouling coating, which involves: (A) obtaining a nano material, a monomer, and an initiator, and mixing the nano material, the monomer, and the initiator to obtain a mixture; and (B) obtaining solvent, and adding the mixture dropwise to the solvent at a temperature of 60-80 degrees C under a protective gas atmosphere, and obtaining a low surface energy antifouling coating.