• 专利标题:   Mouse material comprises polycarbonate, polyphenylene sulfide, graphene, nano-titanium dioxide, nano-silica, modified attapulgite clay, shale diatomaceous earth, antibacterial agent, filler, antioxidant, and coupling agent.
  • 专利号:   CN107227013-A
  • 发明人:  
  • 专利权人:   HEFEI JINHE INFORMATION TECHNOLOGY CO
  • 国际专利分类:   C08K013/06, C08K003/04, C08K003/22, C08K003/34, C08K003/36, C08K005/00, C08L069/00, C08L081/02
  • 专利详细信息:   CN107227013-A 03 Oct 2017 C08L-069/00 201802 Pages: 9 Chinese
  • 申请详细信息:   CN107227013-A CN10625619 27 Jul 2017
  • 优先权号:   CN10625619

▎ 摘  要

NOVELTY - A mouse material comprises 40-60 pts. wt. polycarbonate, 20-50 pts. wt. polyphenylene sulfide, 0.6-1.3 pts. wt. graphene, 8-15 pts. wt. nano-titanium dioxide, 10-17 pts. wt. nano-silica, 9-16 pts. wt. modified attapulgite clay, 5-10 pts. wt. shale diatomaceous earth mud, 10-15 pts. wt. antibacterial agent, 15-20 pts. wt. filler, 3-9 pts. wt. antioxidant, and 2-5 pts. wt. coupling agent. USE - Mouse material (claimed). ADVANTAGE - The mouse material has high waterproof and mechanical properties, high anti-bacterial and anti radiation effect, and wide application range. DETAILED DESCRIPTION - A mouse material comprises 40-60 pts. wt. polycarbonate, 20-50 pts. wt. polyphenylene sulfide, 0.6-1.3 pts. wt. graphene, 8-15 pts. wt. nano-titanium dioxide, 10-17 pts. wt. nano-silica, 9-16 pts. wt. modified attapulgite clay, 5-10 pts. wt. shale diatomaceous earth mud, 10-15 pts. wt. antibacterial agent, 15-20 pts. wt. filler, 3-9 pts. wt. antioxidant, and 2-5 pts. wt. coupling agent. The antibacterial agent comprises 10-20 pts. wt. Artemisia argyi leaves, 15-25 pts. wt. tree peony bark, 10-20 pts. wt. Acorus calamus, 10-15 pts. wt. gallnut, 5-12 pts. wt. indigowoad leaves, 15-22 pts. wt. licorice, 10-15 pts. wt. Angelica, 5-12 pts. wt. Euphorbia, 6-10 pts. wt. cloves and 5-10 pts. wt. Salvia officinalis. An INDEPENDENT CLAIM is included for preparation of mouse material, which involves crushing disinfectant to particle size of less than 300 nm, mixing, adding mixed powder to Soxhlet extractor, extracting with ethanol and water mixed solvent at 78-80 degrees C for 3-5 hours, concentrating extract, freezing and removing the solvent to obtain sterilization freeze-dried powder, adding polycarbonate and polyphenylene sulfide to the reactor, heating to a molten state, adding graphene and coupling agent to the mixture, stirring the reaction for 1-2 hours, adding antioxidant to the reaction mixture, stirring for 10-30 minutes to obtain mixture (a1), adding modified attapulgite clay , shale diatomaceous earth mud and fillers to the mixture (a1), mixing, transferring mixture to shear machine at 500-700 rpm speed, shear dispersing for 10-30 minutes to obtain mixture (a2), adding antibacterial agent to the mixture (a2), mixing ultrasonically treating for 20-30 minutes, adding mixture to twin-screw extruder with screw speed of 330 rpm, melt extruding, and pelletizing.