▎ 摘 要
NOVELTY - Preparation of graphene/fiber fabric, involves steeping fiber fabric in 1-20 mg/ml cattle germ protein solution at room temperature, washing with deionized water, drying to obtain cationic fiber fabric, chemically treating the fiber fabric with a graphene oxide solution by soaking, drying to obtain graphene oxide/fiber fabric, soaking the material in a reducing agent, washing with deionized water, and drying. USE - Preparation of graphene/fiber fabric for sensors (all claimed). ADVANTAGE - The method enables simple preparation of safe and environmentally-friendly graphene/fiber fabric having stable electrical resistance and high sensitivity.