• 专利标题:   Preparing glassware involves taking boron silicon, titanium, quartz grain, phosphorus, metasilicate, feldspar, white plant, sodium nitrate, kyanite, graphene, powder, sodium, cobalt oxide and titanium powder.
  • 专利号:   CN104478216-A
  • 发明人:   HOU J
  • 专利权人:   XIAMEN LONGWEI GLASS PROD CO LTD
  • 国际专利分类:   C03B019/04, C03C001/00, C03C006/06
  • 专利详细信息:   CN104478216-A 01 Apr 2015 C03C-006/06 201540 Pages: 6 Chinese
  • 申请详细信息:   CN104478216-A CN10661102 19 Nov 2014
  • 优先权号:   CN10661102

▎ 摘  要

NOVELTY - Glassware preparation involves taking 32-42 kg boron silicon, 18-22 kg titanium, 310-340 kg quartz grain, 7-10 kg phosphorus, 2-4 kg metasilicate, 54-56 kg feldspar, 2-3 kg white plant, 19.5-21.5 kg sodium nitrate, 3.06-3.26 kg kyanite, 14-16 kg graphene, 4.6-6.5 kg powder, 4.8-6.8 kg sodium, 1.2-3.2 kg cobalt oxide and 7.85-9.85 kg titanium powder. The obtained raw materials are added in a melting furnace. The mixture is heated. The heated mixture is molded. The molded mixture is polished. The molded mixture is annealed at 500-600 degrees C. USE - Method for preparing glassware (claimed). ADVANTAGE - The method enables to prepare glassware in an efficient manner.