▎ 摘 要
NOVELTY - Lithium-philic porous material, is claimed. The porous material has a porous network structure formed by interweaving skeleton materials with lithium-philic modification layers, where the framework material with a lithium-philic modification layer includes a crystalline carbonaceous material that supports the framework, and a lithiophilic modification layer covering at least part of the surface of the crystalline carbonaceous material, where the lithophilic modification layer is made up of amorphous material; at least one of metal complex and metal complex. USE - Used as lithium-philic porous material. ADVANTAGE - The porous material: has strong lithiophilic modification layer; can quickly and completely infiltrate with molten metal lithium; and has no stratification and no pores inside the material. The method can realize industrial production. DETAILED DESCRIPTION - Lithium-philic porous material, is claimed. The porous material has a porous network structure formed by interweaving skeleton materials with lithium-philic modification layers, where the framework material with a lithium-philic modification layer includes a crystalline carbonaceous material that supports the framework, and a lithiophilic modification layer covering at least part of the surface of the crystalline carbonaceous material, where the lithophilic modification layer is made up of amorphous material, and the amorphous material is of formula (CxMyOz); at least one of metal complex of formula (1) and metal complex of formula (2). M = boron, nitrogen, phosphorus, sulfur or halo; x = 3-200; y = 1-50; z = 0-200; and R1, R2, R3, R4 = 1-20C alkyl (at least one hydrogen atoms replaced by oxygen or M). An INDEPENDENT CLAIM is included for preparation of lithium-philic porous material. The method utilizes organic binder, filler, crosslinking agent and solvent, where the filler is crystalline carbonaceous material, organic filler and optional inorganic filler.