▎ 摘 要
NOVELTY - The preparation method of graphene in-situ polymerization modified polyamide 6 pre-oriented yarn involves melt spinning graphene in-situ polymerization modified polyamide 6 slices at winding speed of 3500-4500 m/minute, preferably 3700-4300 m/minute and cooling. USE - The method is useful for preparing graphene in-situ polymerization modified polyamide 6 pre-oriented yarn (claimed). ADVANTAGE - The method enables preparation of graphene in-situ polymerization modified polyamide 6 pre-oriented yarn with excellent tensile strength and elongation rate of 35-45%. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for graphene in-situ polymerization modified polyamide 6 pre-oriented yarn prepared by the method.