▎ 摘 要
NOVELTY - A special aerogel mixed slurry comprises 5-25 %mass aerogel powder, 20-30 %mass adhesive, 5-10 %mass viscosity enhancer, 5-25 %mass titanium dioxide and 25-35 %mass distilled water. The viscosity of the aerogel mixed slurry is 800-3500 cps. USE - Special aerogel mixed slurry used for framing particle board (claimed) used in furniture manufacture and building industry and train and automobile carriage manufacture. ADVANTAGE - The special aerogel mixed slurry has flame retardance, fireproof, heat preserving, adsorption and coating performance of harmful gas and substance, can directly replace the original urea formaldehyde, phenolic resin adhesive. The prepared particle board has high density (0.8-1.3 g/m3), fireproof inflaming retarding, sound absorbing and sound insulation performance, heat preserving and heat insulation effect, and is green, environmentally-friendly, and safe. DETAILED DESCRIPTION - INDEPENDENT CLAIMS are included for the following: 1. preparation of special aerogel mixed slurry, which involves mixing aerogel powder, an adhesive, a viscosity enhancer, titanium dioxide and distilled water and stirring; and 2. a partilce board, which is prepared by preparing materials, chipping, slicing, drying, selecting, mixing glue, paving, pre-pressing, crosscutting, mounting plate, hot pressing, unloading plate, cooling, sawing, checking and storing.